矿物掺合料再生混凝土超声回弹法测强曲线试验
详细信息 本馆镜像全文    |  推荐本文 | | 获取馆网全文
摘要
通过对再生粗骨料取代率为60%,分别掺入矿粉、粉煤灰以及矿粉与粉煤灰(1∶1)双掺为10%,20%,30%的混凝土试件进行抗压强度试验,应用超声回弹检测其抗压强度,推出了超声回弹测强回归式,推动了再生混凝土无损检测技术的研究发展。
The paper undertakes the compressive strength test on the concrete specimen by mixing the mineral powder,the fly ash,and the mineral powder and fly ash(1∶ 1) whose the double mixing are respectively 10%,20% and 30%,and replacement ratio of regenerated coarse aggregate is 60%,adopts the supersonic rebound method to test its compressive strength,points out the strength-measuring regression equation,and the research development of the nondestruction test of the regenerated concrete.
引文
[1]HASSAN K E,CABRERA J G,MALIEHE R S.The effect ofmineral ad-mixtures on the properties of high-performance con-crete[J].Cement and Concrete,2000(22):267-271.
    [2]侯宝隆,蒋之峰.混凝土的非破损检测[M].北京:地震出版社,1992.
    [3]国家建筑工程质量监督检测中心.混凝土无损检测技术[M].北京:中国建材工业出版社,1996.
    [4]TOPCU I B.Physical and mechanical properties of concrete pro-duced with waste concrete[J].Cement and Concrete Research,1997,27(12):1817-1823.
    [5]季光耀.超声回弹综合法检测再生混凝土抗压强度试验研究[J].混凝土,2008(1):122-127.
    [6]陈德玉,袁伟,刘欢.再生骨料取代率及矿物掺合料对混凝土力学性能的影响[J].粉煤灰综合利用,2009(2):14-16.
    [7]孙跃东,肖祥,庞俭,等.再生骨料混凝土的配合比试验研究[J].山东科技大学学报(自然科学版),2009,28(1):25-28.