Voltage Dependent Solid Electrolyte Interphase Formation in Silicon Electrodes: Monitoring the Formation of Organic Decomposition Products
详细信息    查看全文
文摘
The solid electrolyte interphase (SEI) passivating layer that grows on all battery electrodes during cycling is critical to the long-term capacity retention of lithium-ion batteries. Yet, it is inherently difficult to study because of its nanoscale thickness, amorphous composite structure, and air sensitivity. Here, we employ an experimental strategy using p>1p>H, p>7p>Li, p>19p>F, and p>13p>C solid-state nuclear magnetic resonance (ssNMR) to gain insight into the decomposition products in the SEI formed on silicon electrodes, the uncontrolled growth of the SEI representing a major failure mechanism that prevents the practical use of silicon in lithium-ion batteries. The voltage dependent formation of the SEI is confirmed, with the SEI growth correlating with irreversible capacity. By studying both conductive carbon and mixed Si/C composite electrodes separately, a correlation with increased capacity loss of the composite system and the low-voltage silicon plateau is demonstrated. Using selective p>13p>C labeling, we detect decomposition products of the electrolyte solvents ethylene carbonate (EC) and dimethyl carbonate (DMC) independently. EC decomposition products are present in higher concentrations and are dominated by oligomer species. Lithium semicarbonates, lithium fluoride, and lithium carbonate products are also seen. Ab initio calculations have been carried out to aid in the assignment of NMR shifts. ssNMR applied to both rinsed and unrinsed electrodes show that the organics are easily rinsed away, suggesting that they are located on the outer layer of the SEI.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700