摘要
重庆牛角沱嘉陵江大桥属于三类危桥,需进行维修整治。基于文物桥梁"修旧如旧"的维修原则和给老旧桥梁减重延长寿命的原则,混凝土桥面板和桥面系全部拆除,更换为正交异性钢桥面板,栏杆、路灯、桥头堡等附属与原桥建成时外观一致;对锈蚀杆件和有缺陷的铆钉进行更换和补强;对钢桁梁进行喷砂除锈及防腐涂装;对基础采用小型双壁钢围堰内灌注混凝土整体作为永久结构进行防冲刷处置。该桥维修整治后外观恢复到了1966年时通车时的外貌。
The Jialing River Bridge belongs to the three types of dangerous bridges and needs to be repaired and rectified.Based on the maintenance principle of"repairing the old as the old"and the principle of reducing the weight and life of the old bridges,the concrete bridge deck and the deck system are all removed,replaced by orthotropic steel bridge decks,railings,street lamps,bridgeheads,etc. It is consistent with the appearance of the original bridge; the replacement and reinforcement of corroded rods and defective rivets; sandblasting and rust removal and anti-corrosion coating of steel truss beams; and the use of small double-wall steel cofferdams for concrete foundation Anti-scouring treatment as a permanent structure. After the bridge was repaired and rehabilitated,the appearance was restored to the appearance when it was opened in 1966.
引文
[1]陈艺辉,陈波.重庆嘉陵江牛角沱大桥病害检测与评价[J].公路交通技术,2005(6):91-94.
[2]陈艺辉.重庆嘉陵江牛角沱大桥剩余寿命评估研究[J].西南公路,2005(3):42-44.
[3]唐细彪.某桥正交异性钢桥面板结构受力分析[J].世界桥梁,2015(1):32-37.
[4]常付平,蒋彦征,李鹏.结合钢桁梁正交异性钢桥面板体系研究[J].桥梁建设,2011(6):37-41.
[5]张洪双.铆接工艺参数分析[J].机械设计与制造,2011(6):241-243.
[6]李伟,金博.公铁两用钢桁梁铁路桥伸缩缝纵梁节点板更换施工[J].世界桥梁,2014,42(6):85-88.
[7]吕汉中,林世友,严伟鸿,等.停缓建超高层钢结构工程续建时现场大体量喷砂除锈施工工艺[J].钢结构,2012(4):69-75.
[8]王贵春,皇甫昱.桥梁深水基础双壁钢围堰施工技术分析[J].铁道建筑,2007(8):22-24.
[9]郑育林,江小鹏.重庆嘉陵江大桥深水基础双壁钢围堰设计与计算[J].施工技术,2012(12):137-141.