Occurrence of Zinc and Lead in Aerosols and Deposits in the Fluidized-Bed Combustion of Recovered Waste Wood. Part 1: Samples from Boilers
详细信息    查看全文
文摘
Combustion of recovered waste wood (RWW) has led to increased fouling and corrosion of furnace walls, superheaters, and economizers. These problems have been associated mainly with chlorine, zinc, and lead in the deposits but also with sodium and titanium. The presence of lead and zinc compounds, especially lead and zinc chlorides, has been shown to increase the corrosivity of the deposits even at relatively low metal temperatures (230鈭?50 掳C). The present work determined experimentally the distribution and speciation of zinc and lead compounds in aerosol particles and deposits in the fluidized-bed combustion of RWW. Measurements were conducted in both a full-scale (20 MWth) plant with as-received RWW and in a pilot-scale (2 MWth) setup with as-received RWW and RWW doped with zinc and lead. The results show that the amount and speciation of zinc and lead in the deposits vary depending upon the fuel composition, flue gas temperature, and metal temperature. Both lead and zinc chlorides are found in temperature ranges typical for the primary superheater area. A caracolite-type compound [Na3Pb2(SO4)3Cl] was identified in deposits from the economizer area and K2ZnCl4 in the sub-micrometer aerosol particle fraction.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700