CoWO4 nanoparticles prepared by facile sonochemical method.
Spherical morphology with 20–30 nm particle size is obtained.
Antiferromagnetic transition temperature is observed at 20 K.
Curie temperature (−47.6 K) and Curie constant (7.2 K emu mol−1) calculated from Curie-Weiss fitting.